Aluminum Alloys
|
|
A380
|
A360
|
|
|
|
Ultimate Tensile Strength: psi x 103 (MPa)
|
47 |
46 |
Yield Strength -0.2% Offset: psi x 103 (MPa)
|
23 |
24 |
Elongation: % in 2"
|
4 |
5 |
Shear strength: psi x 103 (MPa)
|
30 |
29 |
Hardness: Brinell
|
75 |
|
Impact strength: ft-lb (J)
|
3 |
|
Fatigue Strength Rotary Bend - 5x10 8 cycles
psi x 103 (MPa)
|
20 |
18 |
Compressive Yield strength: 0.1% offset
psi x 103 (MPa)
|
|
|
Modules of elasticity: psi x 103 (MPa)
|
|
|
|
|
|
Physical Properties
|
|
|
Density lb/cu in (gm/cc)
|
1.098 |
0.095 |
Melting Range - Fahrenheit
|
1000-1100 |
1035-1105 |
Melting Range - Centigrade
|
|
|
Electrical Conductivity: % IACS
|
27 |
30 |
Thermal Conductivity: BTU/ft/hr/degree Fahrenheit (W/m/hr/degree Centigrade)
|
55.6 |
70.15 |
Coefficient of thermal expansion
|
11.6 (22) |
|
Specific heat
|
|
|
Pattern shrinkage: inches
|
0.006 |
0.006 |
|
|
|
Chemical Specifications
|
|
|
AL |
Balance |
Balance |
ZN |
2.90 |
0.40 |
Mg |
.10 |
0.45-0.60 |
Cu |
3.0-4.0 |
0.60 |
Fe (max) |
1.3 |
1.3 |
Pb (max) |
|
|
Cd (max) |
|
|
Sn (max) |
.30 |
0.15 |
Ni |
0.50 |
0.50 |
Si |
7.5-9.5 |
9.0-10.0 |
|
|
|
Industry Standard
|
|
|
ASTN |
SC84A |
SG100A |
SAE |
306 |
309 |